1/2" Fiber Board for mold making, fusing, etc. Last for many firings when soaked in Fiber Hardener.
NOTES ON USE:
Fiber board will last longer when fiber hardner is applied. Apply a with brush. Make sure the board is wet to at least 1/4".
Dry before using. You can use a kiln set to 500 deg. F. to dry. Be sure to vent
the area well, since the fumes are profuse
Add as many thickness as you need and then carve your design into the fiber board.
Examples
Mold for glass duck inlay plate
Finished glass piece
Mold for glass boat
(Notice nails hold the layers together)